| 项目 | 参数 | |||
| RN-42 | RN-40 | RN-36 | ||
| Al2O3% | ≥42 | ≥40 | ≥36 | |
|
耐火度℃ |
≥ | 1750 | 1730 | 1690 |
| 1410 | 1350 | 1300 | ||
| 重烧线变化率% | 1450℃x2h | 0~-0.4 | ||
| 1350℃x2h | 0~-0.3 | 0~-0.3 | ||
| 显气孔率% | ≤24 | ≤24 | ≤25 | |
| 常温耐压强度MPa | ≥29.4 | ≥24.5 | ≥19.6 | |
| 项目 | 参数 | |
| ZGN-42 | GN-42 | |
| Al2O3 | ≥42 | ≥42 |
| Fe2o3 | ≤1.7 | ≤1.7 |
|
|
1750 | 1750 |
| 1450 | 1430 | |
| 重烧线变化率 | 0~-0.2 | 0~-0.3 |
| 显气孔率 | ≤15 | ≤16 |
| 常温耐压强度 | ≥58.8 | ≥49 |